Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Syncure™ S1044B Polyethylene, Crosslinked (XLPE)

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer PolyOne Corporation
Trade Name Syncure™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Syncure™ S1044B Polyethylene, Crosslinked (XLPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available as Catalyst Masterbatch component for PolyOne Syncure System.Gel values are >70, and were measured on a 90 phr S1054A / 10 phr S1044B Syncure System; and cured for 8 hours in steam. Pellet appearance is 1/8 Black Beads.Information provided by PolyOne
Physical Properties Metric English Comments
Density 0.600 g/cc
0.0217 lb/in³
Geon® 1169; Internal Method
1.02 g/cc
0.0368 lb/in³
ASTM D1505
Melt Flow 1.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Descriptive Properties Value Comments
Appearance Black
Pellets/Cubes
ASTM D2090
Forms Pellets
Gel Content 70%
ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic Material XLPE
Generic Name Polyethylene, Crosslinked (XLPE)
Regional Availability North America
Retention of Tensile Elongation 90%
121°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength 95%
121°C, 1.91 mm; 168 hr, UL Standard
Uses Wire & Cable Applications
Users viewing this material also viewed the following: