Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Stat-Tech™ PP-CP1/000 HF6 Black Polypropylene Impact Copolymer (PP Impact Copolymer)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer PolyOne Corporation
Trade Name Stat-Tech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ PP-CP1/000 HF6 Black Polypropylene Impact Copolymer (PP Impact Copolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.2 MPa
3800 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1.72 GPa
249 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 1.72 GPa
249 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
Surface Resistance 10000 ohm
10000 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 204 - 238 °C
399 - 460 °F
Mold Temperature 37.8 - 60.0 °C
100 - 140 °F
Descriptive Properties Value Comments
Appearance Black
Features Electrically Conductive
High Flow
Forms Pellets
Generic Material PP Impact Copolymer
Generic Name Polypropylene Impact Copolymer (PP Impact Copolymer)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Medical/Healthcare Applications