Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low to high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.011 - 0.012 cm/cm
0.011 - 0.012 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.021 - 0.022 cm/cm
0.021 - 0.022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.2 MPa
9460 psi
ASTM D638
Elongation at Break 11 %
11 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.13 GPa
454 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.656 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Static Decay 0.0020 sec
0.0020 sec
(Mil-B-81705C), 12% RH, 5000kV to 50kV
Shielding Effectiveness 10 dB

@Frequency 5.00e+9 Hz
10 dB

@Frequency 5.00e+9 Hz
1/8 thickness
11 dB

@Frequency 1.00e+10 Hz
11 dB

@Frequency 1.00e+10 Hz
1/8 thickness
Descriptive Properties Value Comments
Features Electromagnetic Shielding (EMI)
Filler / Reinforcement Stainless Steel Fiber
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Aerospace Applications
Automotive Electronics
Computer Components
Connectors
Electrical Housing
Electrical/Electronic Applications
Copyright © lookpolymers.com All Rights Reserved