Material Notes:
This OnFlex™-S HS thermoplastic elastomer compounds is based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver high strength and medium-low density in addition to typical OnFlex™-S properties such as a wide hardness range, good mechanical properties, good processability, good colourability and a wide temperature operating range.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength at Break 7.20 MPa

@Thickness 2.00 mm
1040 psi

@Thickness 0.0787 in
Flow Injection molded; ISO 37
10.9 MPa

@Thickness 2.00 mm
1580 psi

@Thickness 0.0787 in
FlowExtruded; ISO 37
11.1 MPa

@Thickness 2.00 mm
1610 psi

@Thickness 0.0787 in
Across Flow Injection molded; ISO 37
Elongation at Break 420 %

@Thickness 2.00 mm
420 %

@Thickness 0.0787 in
Flow Injection molded; ISO 37
560 %

@Thickness 2.00 mm
560 %

@Thickness 0.0787 in
Across Flow Injection molded; ISO 37
590 %

@Thickness 2.00 mm
590 %

@Thickness 0.0787 in
FlowExtruded; ISO 37
Processing Properties Metric English Comments
Zone 1 170 °C
338 °F
Zone 2 180 °C
356 °F
Zone 3 190 °C
374 °F
Die Temperature 190 - 200 °C
374 - 392 °F
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Descriptive Properties Value Comments
Features General Purpose
High Strength
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Fast
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Pipe Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliances
Automotive Applications
Consumer Applications
General Purpose
Industrial Applications