Material Notes:
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part performance. These materials have been specifically formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Water Absorption 0.80 %

@Thickness 3.18 mm
0.80 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 110 MPa
16000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 7.58 GPa
1100 ksi
ASTM D638
Flexural Strength 172 MPa
24900 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.693 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C

@Thickness 3.18 mm
399 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Additive Heat Stabilizer
Appearance Grey
Features General Purpose
Filler / Reinforcement GlassMineral, 40% Filler by Weight
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications