PolyOne Nanoblend™ MB 1201 Polypropylene Impact Copolymer (PP Impact Copolymer)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer PolyOne Corporation
Trade Name Nanoblend™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nanoblend™ MB 1201 Polypropylene Impact Copolymer (PP Impact Copolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nanoblend™ Concentrates are highly-filled additive concentrates designed to enhance the properties of thermoplastic compounds. These concentrates can be used to increase flexural modulus, melt strength and tensile yield in compounds containing resins such as polyolefins, polyamides, etc. Additional property enhancements can include lower heat seal strengths, harder surfaces, higher coefficient of friction, higher haze/lower clarity. In some cases, controlled release mechanism or enhanced barrier properties can be achieved. The carrier for the concentrate should be selected to be compatible with the thermoplastic matrix resin to be used in making the compound.Nanomer® is a registered trademark of Nanocor® Inc. Suggested usage level is 10 to 20 weight percent of the Nanoblend™ concentrate.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Descriptive Properties Value Comments
Appearance Brown
Forms Pellets
Generic Material PP Impact Copolymer
Generic Name Polypropylene Impact Copolymer (PP Impact Copolymer)
Nanomer® Level 38 to 42%
Regional Availability North America
South America