Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ FR PP 600 Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR PP 600 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.9 MPa
3760 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 150 %
150 %
Type I, 51 mm/min; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Gardner Impact 15.8 J

@Thickness 3.18 mm,
Temperature 23.0 °C
11.7 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C

@Thickness 3.18 mm
200 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 3.18 mm
HB

@Thickness 0.125 in
NC; UL 94
Descriptive Properties Value Comments
Features Flame Retardant
High Impact Resistance
Low Flow
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Blow Molding
Regional Availability Africa & Middle East