Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam® FR PE 125 Low Density Polyethylene, Wire and Cable  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam® FR PE 125 Low Density Polyethylene, Wire and Cable  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.8 MPa

@Thickness 3.17 mm
2000 psi

@Thickness 0.125 in
2"/min speed; ASTM D638
Elongation at Break 500 %

@Thickness 3.17 mm
500 %

@Thickness 0.125 in
2"/min speed; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Flammability, UL94 V-2

@Thickness 1.59 mm
V-2

@Thickness 0.0625 in
Oxygen Index 24.8 %
24.8 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.32

@Frequency 1000 Hz
2.32

@Frequency 1000 Hz
ASTM D150
2.34

@Frequency 1e+6 Hz
2.34

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00030

@Frequency 1000 Hz
0.00030

@Frequency 1000 Hz
ASTM D150
0.0010

@Frequency 1e+6 Hz
0.0010

@Frequency 1e+6 Hz
ASTM D150