Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ DP-9162-3 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 230 °C
34 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.2 MPa
3800 psi
Type I, 51 mm/min; ASTM D638
Tensile Modulus 1.17 GPa
170 ksi
Type I, 51 mm/min; ASTM D638
Izod Impact, Notched 0.270 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.506 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.3 °C

@Thickness 3.18 mm
155 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 16.0 - 50.0 °C
60.8 - 122 °F
Descriptive Properties Value Comments
Features General Purpose
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: