PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), PTFE Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.022 cm/cm

@Thickness 3.17 mm
0.022 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 47.0 MPa
6820 psi
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm

@Thickness 6.35 mm
0.899 ft-lb/in

@Thickness 0.250 in
ASTM D256
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 238 - 260 °C
460 - 500 °F
Stock
Mold Temperature 49.0 - 93.0 °C
120 - 199 °F
Drying Temperature 82.0 - 93.0 °C
180 - 199 °F