PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612 with PTFE Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 7.0 - 10 %
7.0 - 10 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
ASTM D638
Izod Impact, Notched 0.430 J/cm

@Thickness 6.35 mm
0.806 ft-lb/in

@Thickness 0.250 in
ASTM D256
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 249 - 271 °C
480 - 520 °F
Stock
Mold Temperature 49.0 - 82.0 °C
120 - 180 °F
Drying Temperature 82.0 °C
180 °F