Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Water Absorption 0.010 %

@Thickness 3.17 mm
0.010 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 8.0 %
8.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+17 ohm
1.00e+17 ohm
ASTM D257
Users viewing this material also viewed the following: