PolyOne Geon™ Vinyl Wire & Cable WJJC32L Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable WJJC32L Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
15 sec; ASTM D2240
Tensile Strength at Break 14.8 MPa
2150 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 290 %
290 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
UL Temperature Rating
Brittleness Temperature -26.0 °C
-14.8 °F
ASTM D746
Oxygen Index 39 %

@Thickness 1.91 mm
39 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 174 - 182 °C
345 - 360 °F
Descriptive Properties Value Comments
Agency Ratings UL QMTT2
Features Flame Retardant
Sunlight Resistant (720 hours)
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 82%
100°C, 1.91 mm; 240 hr, UL Standard
RoHS Compliance RoHS Compliant
Uses Communication Wire Jacketing
Wire & Cable Applications
Wire Types CL2
CL2R
CL3R
CMR
FPLR
FT-4
TW