Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable W3400L Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable W3400L Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
15 sec; ASTM D2240
Tensile Strength, Yield 13.8 MPa
2000 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.00862 GPa
1.25 ksi
Type IV, 51 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
UL Temperature Rating
Brittleness Temperature -36.0 °C
-32.8 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
BK; UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
WT; UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
YL; UL 94
V-0

@Thickness 1.90 mm
V-0

@Thickness 0.0748 in
ALL; UL 94
Oxygen Index 27 %

@Thickness 1.91 mm
27 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 182 - 188 °C
360 - 370 °F
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 90%
100°C, 889.0 µm; 240 hr, UL Standard
Retention of Tensile Strength 100%
100°C, 889.0 µm; 240 hr, UL Standard
RoHS Compliance RoHS Compliant
Uses Flexible Cord Jacketing
Wire & Cable Applications
Users viewing this material also viewed the following: