Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable MAF110A Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable MAF110A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
15 sec; ASTM D2240
Tensile Strength, Yield 21.6 MPa
3130 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 290 %
290 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
UL Temperature Rating
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Flammability, UL94 HB

@Thickness 0.500 mm
HB

@Thickness 0.0197 in
ALL; Internal Method
V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
WT; UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
BK; UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
NC; UL 94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
ALL; UL 94
Processing Properties Metric English Comments
Melt Temperature 171 - 182 °C
340 - 360 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL QMFZ2
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Wire & Cable Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved