Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable 3701-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable 3701-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
15 sec; ASTM D2240
Tensile Strength, Yield 17.7 MPa
2570 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 360 %
360 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746
Flammability, UL94 V-2

@Thickness 1.30 mm
V-2

@Thickness 0.0512 in
NC; UL 94
V-2

@Thickness 1.30 mm
V-2

@Thickness 0.0512 in
WT; UL 94
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
BK; UL 94
V-0

@Thickness 2.80 mm
V-0

@Thickness 0.110 in
ALL; UL 94
Oxygen Index 28 %

@Thickness 1.91 mm
28 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 168 - 174 °C
334 - 345 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Features Flame Retardant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Wire & Cable Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved