Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable 1725-xx13FRD Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable 1725-xx13FRD Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
15 sec; ASTM D2240
Tensile Strength, Yield 14.5 MPa
2100 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
UL Temperature Rating
Brittleness Temperature -26.0 °C
-14.8 °F
ASTM D746
Oxygen Index 25 %

@Thickness 1.91 mm
25 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 168 °C
334 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL 719
UL 854
UL QMTT2
Features Flame Retardant
General Purpose
Sunlight Resistant (300 hours)
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 85%
100°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength 100%
100°C, 1.91 mm; 168 hr, UL Standard
Uses Building Wire Jacketing
Cable Jacketing
General Purpose
Wire & Cable Applications
Wire Types NMC
TW
UF
Users viewing this material also viewed the following: