Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
15 sec; ASTM D2240
Tensile Strength, Yield 50.1 MPa
7270 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.70 GPa
392 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.68 GPa
389 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
4.30 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
8.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
12.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
22.5 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy 67.6 J/cm

@Temperature 23.0 °C
0.127 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 74.0 µm/m-°C
41.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 67.8 °C

@Thickness 3.18 mm
154 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features Food Contact Acceptable
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
PVC Cell Classification 16443
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Piping