PolyOne Geon™ Vinyl Packaging XPL 355GC Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Packaging XPL 355GC Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
ASTM D2240
Tensile Strength, Yield 49.4 MPa
7160 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 55 %
55 %
Type I, 5.1 mm/min; ASTM D638
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Processing Properties Metric English Comments
Mold Temperature 199 - 207 °C
390 - 405 °F
Blow Molding
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features Food Contact Acceptable
High Gloss
Medium Impact Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Blow Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Bottles
Packaging