PolyOne Geon™ Vinyl Flexible FC800 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible FC800 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Inst. Hardness +/- 5 units.; ASTM D2240
Tensile Strength at Break 12.5 MPa
1810 psi
510 mm/min; ASTM D638
Elongation at Break 340 %
340 %
510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -37.2 °C
-35.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
191 - 196 °C
376 - 385 °F
Descriptive Properties Value Comments
Features General Purpose
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose