PolyOne Geon™ Vinyl Flexible F80E Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible F80E Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
15 sec; ASTM D2240
Tensile Strength at Break 15.9 MPa
2310 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 138 - 149 °C
280 - 300 °F
Descriptive Properties Value Comments
Additive Barium-Zinc Stabilizer
Features General Purpose
Good Melt Strength
Low Hardness
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose