PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
15 sec; ASTM D2240
60
60
ASTM D2240
Tensile Strength at Break 8.76 MPa
1270 psi
510 mm/min; ASTM D638
Tensile Strength 3.03 MPa

@Strain 100 %
439 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 460 %
460 %
510 mm/min; ASTM D638
Tear Strength 30.6 kN/m
175 pli
Die C, 510 mm/min; ASTM D624
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.0221 GPa
3.21 ksi
ASTM D1043
0.310 GPa

@Temperature -57.0 °C
45.0 ksi

@Temperature -70.6 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -52.8 °C
-63.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 163 - 168 °C
325 - 334 °F
179 - 188 °C
354 - 370 °F
Descriptive Properties Value Comments
Features General Purpose
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose