PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Interior application for thick & thin gauge profile application.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D1638
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
ASTM D2240
Tensile Strength, Yield 45.9 MPa
6660 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.68 GPa
389 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
Izod Impact, Unnotched 0.700 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.31 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 53.8 J/cm

@Temperature 23.0 °C
0.101 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
102 J/cm

@Temperature 23.0 °C
0.191 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
37.2 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C

@Thickness 3.18 mm
165 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
UL 94
Processing Properties Metric English Comments
Melt Temperature 191 - 204 °C
376 - 399 °F
Descriptive Properties Value Comments
Features Low Gloss
Medium Impact Resistance
Forms Powder
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
Profile Extrusion
PVC Cell Classification 12344
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Interior Parts
Profiles
Users viewing this material also viewed the following: