Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Dry Blend E6001 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Dry Blend E6001 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 38.2 MPa
5540 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.72 GPa
540 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 79.5 MPa
11500 psi
ASTM D790
Flexural Modulus 3.72 GPa
540 ksi
ASTM D790
Dart Drop Total Energy 22.2 J/cm

@Temperature 23.0 °C
0.0416 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
30.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 3.18 mm
162 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 191 - 199 °C
376 - 390 °F
Descriptive Properties Value Comments
Features High Flow
Forms Powder
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
Profile Extrusion
PVC Cell Classification 10264
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Vertical Blinds
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved