Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All physicals were measured on an actual extruded part of a shutter profile.High rate inward foam applications.Density range .55-.70.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.707 g/cc
0.707 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
15 sec; ASTM D2240
Tensile Modulus 1.26 GPa
183 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 33.0 MPa
4790 psi
ASTM D790
Flexural Modulus 1.81 GPa
263 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy 20.9 J/cm

@Temperature 23.0 °C
0.0392 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
178 J/cm

@Temperature 23.0 °C
0.333 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C

@Thickness 3.18 mm
144 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 182 - 191 °C
360 - 376 °F
Descriptive Properties Value Comments
Features Foamable
Forms Cellular
Powder
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Building Materials
Outdoor Applications
Copyright © lookpolymers.com All Rights Reserved