PolyOne Geon™ 140 Series 140X466 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 140 Series 140X466 Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shipping: This resin can be shipped in 45,000 lb bulk trucks and 180,000 lb bulk railcars. Information provided by PolyOne
Physical Properties Metric English Comments
Apparent Bulk Density 0.400 g/cc
0.0145 lb/in³
Geon® 1169
Loss On Ignition 0.10 %
0.10 %
Bagged, Geon® 793
Porosity 0.39 %
0.39 %
Geon® 1094; DOP Porosity; cc/g
Particle Size 110 µm
110 µm
Geon® 812
Particle Mesh Size 120 Mesh
120 Mesh
5%; Geon® 812
230 Mesh
230 Mesh
5%; Geon® 812
Relative Viscosity 1.74 cP
1.74 cP
1% Cyclohexanone
Viscosity Measurement 0.66
0.66
Inherent; ASTM D1243-60-A
Descriptive Properties Value Comments
Features Low Molecular Weight
Forms Powder
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 56
No Standard; Correlation
Polymerization Process Suspension
Processing Method Electrostatic Spray Coating
Fluid Bed Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Electrical/Electronic Applications
Fencing & Decking
Protective Coatings