PolyOne Elastamax™ EG-9072 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ EG-9072 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compounds feature unique high melt flow and shear thinning characteristics compared to conventional TPE materials for enhanced processability in injection molding applicationsInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.878 g/cc
0.878 g/cc
ASTM D792
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 190 °C
24 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
10 sec; ASTM D2240
71
71
ASTM D2240
Tensile Strength at Break 3.59 MPa
521 psi
510 mm/min; ASTM D412A
Tensile Stress 2.62 MPa

@Strain 100 %
380 psi

@Strain 100 %
510 mm/min; ASTM D412A
3.03 MPa

@Strain 200 %
439 psi

@Strain 200 %
510 mm/min; ASTM D412A
3.52 MPa

@Strain 300 %
511 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 450 %
450 %
510 mm/min; ASTM D412A
Tear Strength 26.3 kN/m
150 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Features General Purpose
High Flow
Low Density
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications