PolyOne Edgetek® X AS-40CF/000 Natural SE Acrylonitrile Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® X AS-40CF/000 Natural SE Acrylonitrile Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 80.5 MPa
11700 psi
ASTM D638
Flexural Strength 181 MPa
26300 psi
ASTM D790
Flexural Modulus 16.8 GPa
2440 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.899 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Electrical Properties Metric English Comments
Volume Resistivity <= 530 ohm-cm
<= 530 ohm-cm
ASTM D257
Surface Resistance <= 290 ohm
<= 290 ohm
ASTM D257
Descriptive Properties Value Comments
Features Platable
Filler / Reinforcement Carbon Fiber Reinforcement, 40% Filler by Weight
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America