Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm

@Thickness 3.17 mm
0.0010 - 0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 159 MPa
23100 psi
ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
ASTM D638
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Flexural Yield Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Izod Impact, Notched 1.17 - 1.44 J/cm

@Thickness 6.35 mm
2.19 - 2.70 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 223 °C
433 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 217 °C
423 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 271 - 293 °C
520 - 559 °F
Stock
Mold Temperature 93.0 - 107 °C
199 - 225 °F
Drying Temperature 82.0 - 93.0 °C
180 - 199 °F
Users viewing this material also viewed the following: