Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 10% Glass Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM D638
Tensile Modulus 3.40 GPa
493 ksi
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Izod Impact, Notched 0.800 - 1.33 J/cm

@Thickness 6.35 mm
1.50 - 2.49 ft-lb/in

@Thickness 0.250 in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 282 - 304 °C
540 - 579 °F
Stock
Mold Temperature 71.0 - 93.0 °C
160 - 199 °F
Drying Temperature 104 - 110 °C
219 - 230 °F