PolyOne Edgetek® MLS-XC195C-2 Polysulfone Alloy - ESD Material - Lubricated  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® MLS-XC195C-2 Polysulfone Alloy - ESD Material - Lubricated  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 107 MPa
15500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 6.21 GPa
900 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
ASTM D257
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 332 - 349 °C
630 - 660 °F
Molding