PolyOne Edgetek® ES-40GF/000 Polyethersulfone - 40% Glass Fiber Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 40%Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ES-40GF/000 Polyethersulfone - 40% Glass Fiber Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm

@Thickness 3.17 mm
0.0015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 98
98
ASTM D785
Tensile Strength, Ultimate 152 MPa
22000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 221 MPa
32100 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm

@Thickness 6.35 mm
1.80 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
421 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 354 - 382 °C
669 - 720 °F
Stock
Mold Temperature 121 - 149 °C
250 - 300 °F
Drying Temperature 149 °C
300 °F
Users viewing this material also viewed the following: