PolyOne Edgetek® ES-06CF-09GF/000 GREEN Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications &am

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ES-06CF-09GF/000 GREEN Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications &am.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Water Absorption 0.40 %

@Thickness 3.17 mm
0.40 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 131 MPa
19000 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 7.58 GPa
1100 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 221 °C
430 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
415 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm - 1e+05
10000 ohm-cm - 1e+05
ASTM D257
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 354 - 382 °C
670 - 720 °F
Molding