Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Water Absorption 0.60 %

@Thickness 3.17 mm
0.60 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.1 MPa
13500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 204 - 227 °C
400 - 440 °F
Molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved