Material Notes:
Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where exceptional softness and overmolding to polypropylene is desired New Product. Commercial specifications have not been established. - Adhesion to Polypropylene - Enhanced Flow - Excellent Colorability - Tactile Feel - Ultra SoftColor concentrates with Dynalloy™ OBC8000-T05 as the carrier are most suitable for coloring this product. If a OBC8000-T05 color concentrate carrier is desired, it is important that the chosen color house have underwater pelletization capabilities. Typical loadings for color concentrates are 1% to 5% by weight. Liquid color (pigment, not dye) can be used; white oil carriers are recommended. A high color match consistency can be obtained by using precolored compounds available from GLS. Polypropylene (PP) based color concentrates are not recommended because they lead to poor dispersion and can significantly change the hardness of the material. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polystyrene (PS) or polypropylene (PP). Regrind levels up to 20% can be used with Dynalloy™ OBC8000-T05 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt tempetature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynalloy™ OBC8000-T05 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 0.5 to 3 in/sec 1st Stage - Boost Pressure: 200 to 700 psi 2nd Stage - Hold Pressure: 20% of Boost Hold Time (Thick Part): 1 to 5 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.868 g/cc
0.868 g/cc
ASTM D792
Viscosity 7600 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
7600 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
40000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
40000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore OO 57
57
10 sec; ASTM D2240
Tensile Strength at Break 1.25 MPa

@Temperature 23.0 °C
181 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 0.103 MPa

@Strain 100 %,
Temperature 23.0 °C
14.9 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
0.207 MPa

@Strain 300 %,
Temperature 23.0 °C
30.0 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 1400 %

@Temperature 23.0 °C
1400 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Compression Set 10 %

@Temperature 23.0 °C,
Time 79200 sec
10 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
19 %

@Temperature 40.0 °C,
Time 79200 sec
19 %

@Temperature 104 °F,
Time 22.0 hour
ASTM D395B
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 149 - 171 °C
300 - 340 °F
Middle Barrel Temperature 166 - 188 °C
331 - 370 °F
Front Barrel Temperature 177 - 199 °C
351 - 390 °F
Nozzle Temperature 182 - 216 °C
360 - 421 °F
Melt Temperature 182 - 216 °C
360 - 421 °F
Mold Temperature 15.6 - 32.2 °C
60.1 - 90.0 °F
Back Pressure 0.000 - 0.552 MPa
0.000 - 80.1 psi
Screw Speed 80 - 120 rpm
80 - 120 rpm
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1210
Please contact GLS Thermoplastic Elastomers for a copy of the FDA compliance letter.
Appearance Translucent
Features Good Colorability
Good Flow
Good Processing Stability
Low Hardness
Soft
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Consumer Applications
Flexible Grips
Overmolding
Personal Care
Seals
Transparent or Translucent Parts