PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer PolyOne Corporation
Trade Name Bergamid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
±0.02 g/cm³; DIN 53479
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa

@Temperature 23.0 °C
10900 psi

@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 5.5 %

@Temperature 23.0 °C
5.5 %

@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 6.40 J/cm²

@Temperature -30.0 °C
30.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.240 J/cm²

@Temperature -30.0 °C
1.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 243 °C
469 °F
ISO 3146
Maximum Service Temperature, Air 115 °C
239 °F
Continuous (GTP 50% Tensile); IEC 60216
200 °C
392 °F
Short Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Unannealed; ISO 75-2/A
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
ALL; Internal Method
Glow Wire Test 725 °C

@Thickness 0.800 mm
1340 °F

@Thickness 0.0315 in
uncolored material; Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 0.800 mm
1760 °F

@Thickness 0.0315 in
Flammability Index; uncolored material; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 45.0 kV/mm
1140 kV/in
IEC 60243-1
Dissipation Factor 0.30

@Frequency 1.00e+6 Hz
0.30

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Descriptive Properties Value Comments
Additive Heat Stabilizer
Features Flame Retardant
Good Flow
Halogen Free
Heat Stabilized
Low (to None) Phosphorus Content
Forms Pellets
Generic Material Nylon 66/6
Generic Name Polyamide 66/6 Copolymer (Nylon 66/6)
Regional Availability Africa & Middle East
Asia Pacific
Europe
RoHS Compliance RoHS Compliant