Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.40 g/cc

@Temperature 23.0 °C
0.0506 lb/in³

@Temperature 73.4 °F
±0.03 g/cm³; DIN 53479
Ash >= 25 %
>= 25 %
ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa

@Thickness 4.00 mm,
Temperature 23.0 °C
18100 psi

@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/5
Elongation at Break >= 2.0 %

@Temperature 23.0 °C
>= 2.0 %

@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 8.00 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
1160 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/1
Charpy Impact Unnotched 5.50 J/cm²

@Temperature -30.0 °C
26.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 261 °C
502 °F
ISO 3146
Maximum Service Temperature, Air 120 °C
248 °F
Continuous (GTP 50% Tensile); IEC 60216
220 °C
428 °F
Short Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Unannealed; ISO 75-2/B
Flammability, UL94 V-0

@Thickness 0.800 - 3.00 mm
V-0

@Thickness 0.0315 - 0.118 in
ALL; UL 94
Glow Wire Test 750 °C

@Thickness 1.60 mm
1380 °F

@Thickness 0.0630 in
Ignition Temperature; IEC 60695-2-13
775 °C

@Thickness 3.00 mm
1430 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 0.800 - 3.00 mm
1760 °F

@Thickness 0.0315 - 0.118 in
Flammability Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index >= 400 V
>= 400 V
Solution A; IEC 60112
Descriptive Properties Value Comments
Additive Heat Stabilizer
Features Flame Retardant
Halogen Free
Heat Stabilized
High Impact Resistance
Filler / Reinforcement Glass Fiber Reinforcement, 25% Filler by Weight
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Regional Availability Europe
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: