Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen RP210R Extrusion Coating and Lamination Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen RP210R Extrusion Coating and Lamination Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen RP210R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP210R is a copolymer particularly suitable for extrusion coating and lamination of flexible film packaging. Moplen RP210R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Low neck-in and high speed; Adhesion to OPP substrate; Heat seal performanceApplications: Flexible film packaging (OPP)Information provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 21.6 MPa
3130 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 0.785 GPa
114 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525