Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HP563S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP563S is a homopolymer typically used in spunbonded nonwovens. Moplen HP563S resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.Features: Excellent spinnability; Excellent drawability; Anti-gas fadingApplications: Diaper and Sanitary Napkin; Agriculture; Shopping Bag; Apparel Cover; Wet TissuesInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 38 g/10 min

@Load 2.16 kg,
Temperature 230 °C
38 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 37.3 MPa
5400 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648