Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HP552R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552R is a homopolymer typically used by customers in high speed production of staple fiber. Moplen HP552R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.Features: Excellent spinnability; Excellent drawability; Anti-gas fading; Outstanding gloss and surface appearanceApplications: Staple Fiber for diaper and sanitary napkin; BCF/Multi-Filament: Automobile Interior stuffs; Industrial; Base resin for Master/BatchInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 37.3 MPa
5400 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ASTM D648
Users viewing this material also viewed the following: