Material Notes:
Moplen HP521M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP521M is suitable for core resin of co-extrusion CPP film. Moplen HP521M resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact. Features: Good processability/Good optical properties/Good Stiffness Applications: General purpose CPP/Metallizable CPP/Food and clothes packagingInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525