Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen EP300R Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP300R Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection molding of washing machine tub, thin-walled packaging, parts of electrical appliances, housewares. Moplen EP300R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Optimized balance of stiffness and toughness; High impact strength even at low temperature; Low warpage and fast cycle time; High stiffnessApplications: Washing machine tub; Parts of electrical appliance; HousewaresInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 23.5 MPa
3410 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Temperature -20.0 °C
0.918 ft-lb/in

@Temperature -4.00 °F
ASTM D256
1.18 J/cm

@Temperature 23.0 °C
2.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Users viewing this material also viewed the following: