PolyMirae Moplen EP200R Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP200R Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP200R is the reactor TPO manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP200R is a super impact copolymer particularly suitable for injection molding of high impact resistance required application and compounding base resin of automotive bumper fascia.Features: Super high impact strength even at low temperature; Improved processabilityApplications: Automotive; High impact resistance required application; ContainerInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Yield 17.7 MPa
2560 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 0.735 GPa
107 ksi
ASTM D790
Izod Impact, Notched 1.27 J/cm

@Temperature -20.0 °C
2.39 ft-lb/in

@Temperature -4.00 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 30 %
30 %
60°; ASTM D523