PolyChem Alloy PolyFast 8167UC

Category Polymer
Manufacturer PolyChem Alloy
Trade Name PolyFast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyChem Alloy PolyFast 8167UC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV Stabilizer Masterbatches For Nylon
Processing Properties Metric English Comments
Processing Temperature 290 - 310 °C
554 - 590 °F
Descriptive Properties Value Comments
Color Off-White