Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer Polimeros Mexicanos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excellent mechanical and environmental resistance properties. Available as black powder.Applications: High quality Polyethylene recommended for producing industrial tanks, cisterns, agricultural tanks, chemical tanks or for applications requiring excellent chemical resistance, impact strength and ESCR resistance. Molded parts have a smooth surface finish. This product contains mold release internal agents which eliminate the application of mold release products in the mold inner surface.The carrier of this product meets all FDA requirements as specified in 21 CFR 177.1520 and CONEG (as a compound), covering safe use in articles for direct food contact.Information provided by Polimeros Mexicanos
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 900 hour
>= 900 hour
ASTM D1693
ESCR 10% Igepal® >= 900 hour
>= 900 hour
ASTM D1693
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
2 in/min; ASTM D638
Tensile Strength, Yield 18.6 MPa
2700 psi
2 in/min; ASTM D638
Elongation at Break >= 900 %
>= 900 %
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
1% Secant; ASTM D790
Impact Test 67.8 J

@Temperature -40.0 °C
50.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM STD test
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Descriptive Properties Value Comments
Process Rotational Molding