Polimeri Europa SINKRAL PD M323 ABS  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa SINKRAL PD M323 ABS  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose injection moulding grade that exhibits outstanding flow and thermal stability during processing. Thanks to its` excellent stability, SINKRAL PD M323 is tailored for applications where the colour constancy of finished articles is essential, such as in the white goods industry.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.0 %
1.0 %
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Humidity Absorption
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 220 °C
35 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
50 mm/min
Elongation at Break 15 %
15 %
Nominal
Elongation at Yield 3.1 %
3.1 %
50 mm/min
Tensile Modulus 2.40 GPa
348 ksi
1 mm/min
Charpy Impact Unnotched 13.0 J/cm²
61.9 ft-lb/in²
10.0 J/cm²

@Temperature -30.0 °C
47.6 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Vicat Softening Point 96.0 °C
205 °F
50°C/hr; 50N
Glass Transition Temp, Tg 105 °C
221 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in
Comparative Tracking Index 600 V
600 V