Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Greenflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Greenflex ML 60 is recommended for the production of foamed and crosslinked sheets for shoes and gaskets.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ISO 1183
Vinyl Acetate Content 28 %
28 %
Internal Method
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ISO 868/A
Hardness, Shore D 32
32
ISO 868/A
Tensile Strength, Yield 3.00 MPa
435 psi
ISO 527
Flexural Modulus 0.0100 GPa
1.45 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 74.0 °C
165 °F
Internal Method
Vicat Softening Point 44.0 °C

@Load 1.00 kg
111 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746