Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL TH 2314 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where bound styrene content is 31%wt. A non-staining, TNPP free antioxidant system is added during the production process.Key Features: Europrene® SOL TH 2314 is a linear triblock copolymer of medium-high molecular weight, designed for technical compound applications. The grade is characterized by excellent processability, mechanical properties and ageing resistance.Main Applications: Europrene® SOL TH 2314 is designed for technical compound applications. High performance compounds base on Europrene® SOL TH 2314 show excellent elastic and tensile characteristics, in a wide range of flowability and hardness. SOL TH 2314 could also be used in polymer modification.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
300% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
Users viewing this material also viewed the following: