Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL T 6414 Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 6414 Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 6414 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 40% weight and diblock content is 22%. A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 6414 is a radial block copolymer, characterized by excellent dispersability, processability and thermo-oxidative resistance, combined with high strength, elongation and hardness.Main Applications: Europrene® SOL T 6414 is designed for hot melt adhesive applications: the grade shows high compatibility with tackifiers and imparts low melt viscosities and an excellent balance of adhesive and cohesive properties to the hot melt products. The grade is also used in footwear compounds, particularly where smooth and glossy surface finishing is required. Characterized by excellent processability, SOL T 6414 is widely used in the modification of polymers and plastic recycling.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Brookfield Viscosity 0.040 cP
0.040 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 190 °C
11 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D2240
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D412
Elongation at Break 850 %
850 %
ASTM D412
300% Modulus 0.00390 GPa
0.566 ksi
ASTM D412