Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL T 6320 Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 6320 Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 6320 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 31% weight and diblock content is 75%. A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 6320 is a linear block copolymer, characterized by excellent dispersability and extremely easy processability.Main Applications: Designed for bitumen modification, where high compatibility and easy dispersability are requested, Europrene® SOL T 6320 provides very low viscosity to bituminous binders. The high diblock content also assures excellent performance in adhesive applications, including bituminous self adhesive membranes. Characterized by excellent processability, SOL T 6320 can be used in polymer modification and plastic recycling.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Brookfield Viscosity 0.060 cP
0.060 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 190 °C
11 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
ASTM D2240
Tensile Strength at Break 6.00 MPa
870 psi
ASTM D412
Elongation at Break 1200 %
1200 %
ASTM D412
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D412